Organic solid-state battery cells can maintain stable cycling at just 1 MPa of external pressure, retaining 80.3% capacity after 100 cycles, according to research published on Wednesday in Nature Communications.
- Researchers used bistetraaminobenzoquinone (TAQ) as a model system in all-solid-state cells.
- The elastic modulus and hardness for pristine TAQ measure 8.4 ± 0.4 GPa and 0.33 ± 0.01 GPa, respectively.
- Lithiated Li4TAQ increases in elastic modulus to 15.3 ± 1 GPa and hardness to 0.76 ± 0.06 GPa.
Organic Cathodes Reduce Pressure Requirements
All-solid-state batteries typically require high external pressure to maintain intimate solid–solid contact and preserve active material particle integrity during operation, iopscience.iop.org reported. The new Nature Communications study demonstrates that organic active materials possess inherent softness and high malleability that enable stable operation under significantly reduced stack pressures.
Investigators Zhaoyang Chen, Alae Eddine Lakraychi, Santosh Thapa and their colleagues characterized the mechanical properties across charge-discharge cycles using nanoindentation, as shown in Fig. 2a. The resulting values sit more than one order of magnitude lower than those reported for oxides. This primes the materials to deform under reasonably low pressures without the heavy external constraints usually needed for inorganic counterparts.
Creep behavior measured across charge states
Nanoindentation displacement curves for both TAQ and Li4TAQ show time-dependent responses under constant load, a hallmark of creep behavior reported in the Nature Communications study. The strain-rate sensitivity exponent was calculated as 0.038 for pristine TAQ and 0.073 for lithiated Li4TAQ, indicating moderate time-dependent deformation. These values align with organic crystals but remain lower than creep-prone materials such as lithium and selenium, which exhibit exponents of 0.1 to 0.3.
Supplementary Fig. 1b and 1c in the source article detail the indentation tests across varying strain rates used to quantify this rate-dependent deformation. The moderate exponents suggest the material can accommodate volume changes during cycling without the high external constraints typically required for inorganic electrodes.
S–S species concentration rises with temperature
The electrochemical profile closely mirrors behavior observed in liquid electrolytes, suggesting a similar intercalation reaction mechanism operates in the solid state.
TAQ-based cathodes achieve an electrode-level specific capacity of 183 mAh g⁻¹, placing them among competitive values reported for oxide-based positive electrodes. This figure appears in Fig. 3d and Supplementary Table 1 of the Nature Communications study, which compares TAQ performance against state-of-the-art inorganic electrode materials.
Structural Integrity Under Low Stack Pressure
Operando scanning electron microscope imaging revealed that TAQ maintains structural integrity without crack formation during cycling. By contrast, inorganic-based single-crystal cathodes frequently develop transverse cracks during the initial charge under low stack pressures.
Nature Communications, a multidisciplinary open-access journal published by Nature Portfolio since 2010, covers physics, chemistry, earth sciences, medicine, and biology from editorial offices in London, Berlin, New York City, and Shanghai. The journal publishes high-quality research representing important advances of significance to specialists across all areas of the natural sciences.
Its reputation is reflected in a 2025 impact factor of 18.1 (Journal Citation Reports), a 2-year impact factor of 15.7 (2024), a 5-year impact factor of 17.2 (2024), and 177,272,701 article downloads in 2024, with a median of 8 days from submission to first editorial decision.
Long-term stability tests across multiple pressure thresholds showed capacity retentions of 86.8%, 88.9%, and 80.3% after 100 cycles under stack pressures of 14 MPa, 2 MPa, and 1 MPa, respectively. Postmortem analysis confirmed that TAQ electrodes cycled under 1 MPa keep an intact morphology with zero cracks or interfacial delamination.
Keep reading